JIN Carbide Drill for Titanium & Superalloy — Shank Type
JIN is the grade we run on titanium, Inconel and other high-temperature alloys — materials that work-harden under the drill point and destroy a general-purpose edge within a few holes. A sharp point, a coated flute and a reduced shank together keep the drill cutting instead of rubbing.
Why a sharper point matters on titanium
Titanium work-hardens the moment an edge rubs instead of cuts. A sharp, narrow point puts less thrust into the material at entry, so the surface does not harden ahead of the cutting edge and the drill keeps biting instead of skating.
Why the coating
Titanium and nickel alloys are chemically sticky. A coated flute sheds the chip instead of welding it to the rake face — that welding is what causes the sudden edge failure people blame on the carbide. The coating also gives a visible wear marker: when it rubs through at the margin, it is time to change the tool.
0.5xD3x5x50 means 0.5 mm drill diameter, 3 mm reduced shank, 5 mm flute, 50 mm overall. The shank stays thick for rigidity while the cutting end goes small — the usual way to drill a deep small hole without snapping the tool.
Running it
Titanium wants low surface speed and high feed per revolution — never let the drill dwell. Use through-tool or flood coolant, peck only as deep as the flute can clear, and keep the drill moving: a stationary edge on titanium work-hardens the hole in under a second.